Degradation of Mg-6Zn alloy stents does not influence the healing of the common bile duct in vivo

Mg-6Zn合金支架降解不影响体内胆管愈合

阅读:11
作者:Yigang Chen, Nianfeng Sun, Jie Zhang, Shaoxiang Zhang, Changli Zhao, Jiazeng Xia

Abstract

To investigate the effects of Mg-6Zn alloy on the healing of the common bile duct (CBD), Mg-6Zn alloy stents were implanted into the CBDs of rabbits. Stainless steel stents were transplanted into a second group of rabbits to serve as a control. Computed tomography (CT) scanning was performed and weight loss was recorded to evaluate the in vivo degradation process. Hematoxylin and eosin staining and immunohistochemical analyses were performed to determine the expressions of transforming growth factor (TGF)-β, vascular endothelial growth factor (VEGF) and basic fibroblast growth factor (bFGF) and evaluate CBD healing. The Mg-6Zn stents maintained ~82 and ~50% of the original length, and ~90 and ~43% of the original CT value at 1 and 2 weeks post-operatively, respectively. The residual weights of the Mg-6Zn stents were ~89, ~42 and ~9% of the original weights at 1, 2 and 3 weeks post-operatively, respectively. At 3 weeks post-surgery, the CBD was completely healed, with no wounds observed in the 3 groups. VEGF expression in the Mg-6Zn stent group was lower than that in the stainless steel stent group at 3 weeks post-surgery (P=0.002). No significant differences were observed between the mean expressions of the TGF-β1 and bFGF genes at 1 and 2 weeks post-surgery. The results of the present study suggest that degradation of the Mg-6Zn alloy may not affect healing of the CBD.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。